The PP non woven fabric used for 3-layer flat mask is generally 25 gram per square meter, and the outer layer of black mask or FFP2 mask is made of 50g non-woven fabric or as required by customers. The layer of spun bond non woven fabric near the face of users is 25g per square meter PP non woven fabric.
The spun bond non-woven fabric is a one-step production of anti adhesion non-woven fabric, which uses polypropylene raw material to melt at high temperature and spin into web, and then hot-rolled after finishing. It weighs 10-150 grams per square meter.
different color PP non woven fabric
TEST REPORT OF SPUN BOND NON WOVEN FABRIC
PRODUCT |
Spun bond non woven fabric |
Specification |
25g SS |
lot |
200329-1-q |
||||
material |
PP |
Product amount |
1602.42 Kgs |
color |
Matte white |
||||
standard |
FZ/T64033-2014 |
Sampling amount |
30 meters |
Test time |
2021.01.25 |
||||
item |
requirement |
result |
conclusion |
||||||
Interior quality |
Width deviation/mm |
±3 |
0 |
qualified |
|||||
Mass deviation rate per unit area /% |
±7.5 |
-7 |
qualified |
||||||
mass variation coefficient of unit area /% |
≤7 |
4.9 |
qualified |
||||||
Breaking strength/N |
longitudinal |
≥33.5 |
34.1 |
qualified |
|||||
transverse |
≥22.5 |
24.2 |
qualified |
||||||
Elongation at break/% |
longitudinal |
≥30 |
152.2 |
qualified |
|||||
transverse |
≥30 |
125.2 |
qualified |
||||||
Appearance quality |
holes more than 4mm2 without fibre in the centre |
Not allowed |
comply |
qualified |
|||||
color difference/grade |
4~5 |
5 |
qualified |
||||||
bad trimming,>4mm |
Not allowed |
comply |
qualified |
||||||
joints(pc/2000m) |
≤1,marked with colored tape |
comply |
qualified |
||||||
frit |
area≥1cm2 |
Not allowed |
comply |
qualified |
|||||
area<1cm2/(pc/1000m) |
≤10 |
comply |
qualified |
||||||
Foreign matter |
Not allowed |
comply |
qualified |
||||||
Poor net laying |
length<5cm/(pc/1000m) |
≤10 |
comply |
qualified |
|||||
5cm≤length≤10cm/(pc/1000m) |
≤5 |
comply |
qualified |
||||||
length>10cm |
Not allowed |
comply |
qualified |
||||||
Soft fold |
length≤30cm/(pc/1000m) |
≤2 |
comply |
qualified |
|||||
length>30cm |
Not allowed |
comply |
qualified |
||||||
Conclusion |
qualified |
||||||||
remarks |
For engineering products, the "foreign matter" index under the "appearance quality" test items shall be implemented according to the contract. |
PP non woven fabric for face mask
Some concepts of non woven cloth
S: Spun bond non woven
M: Melt blown fabric
S: Spun bonded non woven = single layer web hot rolled
SS: spun bond non woven + spun bond non woven = hot rolled from two layers of fiber web
SSS: spun bond non woven + spun bond non woven + spun bond non woven = three-layer web hot rolled
SSSS: spun bond non woven + spun bond non woven + spun bond non woven+ spun bond non woven= four layer web hot rolled
SMS: spun bond non woven + melt blown fabric + spun bond non woven = three-layer web hot rolled
SMMS: spun bond non woven + melt blown fabric + melt blown fabric+ spun bond non woven = four layers of fiber web hot rolled.
PP non woven fabric machine
PP non woven fabric sample
printed PP non woven fabric in roll
printed PP non woven fabric
spun bond non woven fabric roll
storage of PP non woven fabric roll
storage of spun bond non woven fabric roll